SRD-100 microcomputer controlled electronic creep tester
SRD-100 microcomputer-controlled electronic creep tester can perform tensile, creep, long-lasting and stress relaxation tests on metal non-metal materials under certain temperature conditions, and can also perform low cycle fatigue and creep fatigue tests. Mainly used in the measurement of quality inspection, aerospace, metallurgical steel, colleges and universities and research laboratories and other industrial sectors.
Spesification
Serial number |
project name |
Technical Parameters |
1 |
Maximum test force (kN) |
100 |
2 |
level of accuracy |
0.5 level / 1 level |
3 |
Test force measurement range |
1% to 100% FS |
4 |
Test force relative value |
±0.5%/±1% |
5 |
Test force resolution |
1/240000 (no change in the whole range) |
6 |
Concentricity |
≤10% |
7 |
Deformation measurement error |
±0.002mm (grating sensor) |
8 |
Pull rod maximum stroke |
150mm |
9 |
Tie rod speed |
0.01~50mm/min |
10 |
Mainframe dimensions (length × width × height) mm |
820×500×2360 |
11 |
Host weight (kg) |
520 |
12 |
Temperature range (°C) |
200~1100 |
13 |
Temperature fluctuation (°C) |
±2 |
14 |
Average tropical length (mm) |
150 |
15 |
Temperature gradient (°C) |
3 |